規(guī)格級(jí)別 | 其它 其它 吹塑 | 外觀顏色 | |
該料用途 | |||
備注說(shuō)明 |
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | |
基本性能 | 密度 | ASTM D-792 | 0.926 | g/m3 | |
基本性能 | 熔體流動(dòng)速率 | ASTM D-1238 | 1 | g/10min | |
基本性能 | 薄膜厚度 | 38.1 | um | ||
機(jī)械性能 | 割線模量(TD) | 2% Secant,38.1um | ASTM D-882 | 208 | MPa |
機(jī)械性能 | 割線模量(MD) | 2% Secant,38.1um | ASTM D-882 | 190 | MPa |
機(jī)械性能 | 拉伸屈服強(qiáng)度(TD) | 38.1um | ASTM D-882 | 11.2 | MPa |
機(jī)械性能 | 拉伸屈服強(qiáng)度(MD) | 38.1um | ASTM D-882 | 11.4 | MPa |
機(jī)械性能 | 拉伸斷裂強(qiáng)度(MD) | 38.1um | ASTM D-882 | 50.1 | MPa |
機(jī)械性能 | 拉伸斷裂強(qiáng)度(TD) | 38.1um | ASTM D-882 | 41.3 | MPa |
機(jī)械性能 | 拉伸斷裂伸長(zhǎng)率(MD) | 38.1um | ASTM D-882 | 610 | % |
機(jī)械性能 | 拉伸斷裂伸長(zhǎng)率(TD) | 38.1um | ASTM D-882 | 720 | % |
機(jī)械性能 | 落錘沖擊 | 25.4um | ASTM D-1709A | 250 | g |
機(jī)械性能 | 埃爾曼多夫撕裂強(qiáng)度(TD) | 38.1um | ASTM D-1922 | 600 | g |
機(jī)械性能 | 埃爾曼多夫撕裂強(qiáng)度(MD) | 38.1um | ASTM D-1922 | 940 | |
熱性能 | 維卡軟化點(diǎn) | ASTM D-1525 | 106 | ℃ | |
熱性能 | 熔化溫度 | Internal Method | 121 | ℃ | |
其它性能 | 電影穿刺抵抗運(yùn)動(dòng) | 38.1um | Internal Method | 13.8 | J/cm3 |
其它性能 | 電影韌性(TD) | 38.1um | ASTM D-882 | 96.4 | J/cm3 |
其它性能 | 電影韌性(MD) | 38.1um | ASTM D-882 | 93.3 | J/cm4 |
光學(xué)性能 | 光澤度 | 45°,38.1um | ASTM D-2457 | 71 | |
光學(xué)性能 | 霧度 | 38.1um | ASTM D-1003 | 8 | % |