規(guī)格級(jí)別 | 良好的撕裂強(qiáng)度,可加工性,良好,低速凝固晶點(diǎn),低密度,辛烯共聚單體,抗氧化性,食品接觸的合規(guī)性,良好的熱封性,韌性良好 共擠出成型,薄膜擠出 | 外觀顏色 | |
該料用途 | 層壓板,薄膜 | ||
備注說(shuō)明 |
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | |
物理性能 | 比重 | ASTMD792 | 0.917 | g/cm3 | |
物理性能 | 熔流率(熔體流動(dòng)速率)(190°C/2.16kg) | ASTMD1238 | 1.0 | g/10min | |
薄膜 | 薄膜厚度-經(jīng)測(cè)試 | 25 | μm | ||
薄膜 | SecantModulus-1%Secant,MD(25μm,BlownFilm) | ASTMD882 | 126 | MPa | |
薄膜 | SecantModulus-1%Secant,TD(25μm,BlownFilm) | ASTMD882 | 132 | MPa | |
薄膜 | TensileStrength-MD(Yield,25μm,BlownFilm) | ASTMD882 | 9.00 | MPa | |
薄膜 | TensileStrength-TD(Yield,25μm,BlownFilm) | ASTMD882 | 9.00 | MPa | |
薄膜 | TensileStrength-MD(Break,25μm,BlownFilm) | ASTMD882 | 46.0 | MPa | |
薄膜 | TensileStrength-TD(Break,25μm,BlownFilm) | ASTMD882 | 42.0 | MPa | |
薄膜 | TensileElongation-MD(Break,25μm,BlownFilm) | ASTMD882 | 540 | % | |
薄膜 | TensileElongation-TD(Break,25μm,BlownFilm) | ASTMD882 | 760 | % | |
薄膜 | 落錘沖擊(25μm,吹塑薄膜) | ASTMD1709A | 400 | g | |
薄膜 | ElmendorfTearStrength-MD(25μm,BlownFilm) | ASTMD1922 | 300 | g | |
薄膜 | ElmendorfTearStrength-TD(25μm,BlownFilm) | ASTMD1922 | 450 | g | |
薄膜 | SealInitiationTemperature(25μm,BlownFilm) | 100 | °C | ||
光學(xué)性能 | 光澤度 | 45°,25.0μm,BlownFilm2 | ASTMD2457 | 72 | |
光學(xué)性能 | 光澤度 | 45°,25.0μm,BlownFilm3 | ASTMD2457 | 37 | |
光學(xué)性能 | 霧度 | 25.0μm,BlownFilm2 | ASTMD1003 | 7.0 | % |
光學(xué)性能 | 霧度 | 25.0μm,BlownFilm3 | ASTMD1003 | 16 | % |
ADDITIONAL INFORMATION | 補(bǔ)充信息 | TestMethod | NominalValue | Unit | |
ADDITIONAL INFORMATION | LowFrictionPuncture-BlownFilm(25.0μm) | InternalMethod | 790 | J/cm |