性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | |
物理性能 | 密度 | ASTMD1505 | 0.918 | g/cm3 | |
物理性能 | 熔流率(熔體流動(dòng)速率)(190°C/2.16kg) | ASTMD1238 | 1.0 | g/10min | |
薄膜 | 薄膜厚度-經(jīng)測(cè)試 | 25 | μm | ||
薄膜 | 割線模量-1%正割,MD(25μm) | ASTMD882 | 175 | MPa | |
薄膜 | SecantModulus-1%Secant,TD(25μm) | ASTMD882 | 191 | MPa | |
薄膜 | TensileStrength-MD(Yield,25μm) | ASTMD882 | 10.7 | MPa | |
薄膜 | TensileStrength-TD(Yield,25μm) | ASTMD882 | 9.65 | MPa | |
薄膜 | TensileStrength-MD(Break,25μm) | ASTMD882 | 58.6 | MPa | |
薄膜 | TensileStrength-TD(Break,25μm) | ASTMD882 | 51.7 | MPa | |
薄膜 | 伸長(zhǎng)率-MD(斷裂,25μm) | ASTMD882 | 450 | % | |
薄膜 | TensileElongation-TD(Break,25μm) | ASTMD882 | 620 | % | |
薄膜 | DartDropImpact3(25μm) | ASTMD1709 | 760 | g | |
薄膜 | 埃爾曼多夫抗撕強(qiáng)度-MD(25μm) | ASTMD1922 | 230 | g | |
薄膜 | ElmendorfTearStrength-TD(25μm) | ASTMD1922 | 500 | g | |
光學(xué)性能 | 光澤度(60°,25.4μm,吹塑薄膜) | ASTMD2457 | 93 | ||
光學(xué)性能 | 霧度(25.4μm,吹塑薄膜) | ASTMD1003 | 11 | % |